SiO2 | Al2O3 | Fe2O3 | Na2O+K2O |
45%-55% | 40-50% | 0.8%-1.0% | 0.2%-0.5% |
Project | Index(%) |
The average fiber length | 0.15--2.5mm |
The average fiber diameter | 4-9um |
Fiber distribution | D50 |
Specific Gravity | 0.25-0.45g/m3 |
Fiber moisture | ≤1.0 |
Fiber diameter | 2-4um |
Fiber loss-on-ignition | <0.5,(800/H) |
Softening Point | >1750Temperature |
PH | 7 |
Fiber Asbestos Content | 0 |
Shot Content;>120mesh | <20 |
Surface density(state of compression) | 0.13-0.20g/ cm³ |
Project | Index(%) |
The average fiber length | 0--1mm |
The average fiber diameter | 4-9um |
Fiber distribution | D50 |
Specific Gravity | 0.45-0.55g/m3 |
Fiber moisture | ≤1.5 |
Fiber diameter | 2-4um |
Fiber loss-on-ignition | <0.5,(800/H) |
Softening Point | >1750Temperature |
PH | 7 |
Fiber Asbestos Content | 0 |
Shot Content;>120mesh | <30 |
Surface density(state of compression) | 0.25-0.40g/ cm³ |
Project | Index(%) |
The average fiber length | 0.10--2.0mm |
The average fiber diameter | 4-9um |
Fiber distribution | D50 |
Specific Gravity | 0.25-0.35g/m3 |
Fiber moisture | ≤1.0 |
Fiber diameter | 2-4um |
Fiber loss-on-ignition | <0.5,(800/H) |
Softening Point | >1750Temperature |
PH | 7 |
Fiber Asbestos Content | 0 |
Shot Content;>120mesh | <25 |
Surface density(state of compression) | 0.25-0.35g/ cm³ |
Project | Indicators |
Specific Gravity | 2.25g/cm³ |
Fiber length | 1.0-3.5mm |
Loose density | 800-1100 cm³/100g |
105ºC Volatiles | <2.5% |
Slag ball Content | >120mesh; < 2% |
800ºC Burn loss | 28-32% |
Fiber diameter | 3-8μm |
P H | 8-10 |
Main ingredients | Mineral Fiber 70% Cellulose Fiber 30% |